Many contractors make the mistake of using the same grout for every job, leading to callbacks and unhappy clients. The truth is: different cracks demand different solutions.
Scenario 1: Hairline Cracks (0.1-1mm)
Best Choice: Low-viscosity epoxy grout
Why: Penetrates like water into microscopic spaces
Cure Time: 6-8 hours
Application Tip: Use gravity feed injection for complete penetration
Scenario 2: Moving Cracks (Seasonal expansion/contraction)
Best Choice: Flexible polyurethane grout
Why: Moves with the structure (up to 300% elasticity)
Cure Time: 2-4 hours
Application Tip: Over-drill and sleeve injection points to allow movement
Scenario 3: Water-Active Cracks
Best Choice: Hydrophobic polyurethane grout
Why: Expands upon water contact, creating a mechanical lock
Cure Time: 1-3 minutes
Application Tip: Inject during heaviest flow for maximum expansion
Always test grout consistency before injection
Maintain constant pressure between 100-300 PSI
Document injection volumes for future reference
Use UV-stable grouts for exterior applications